Abstract
This chapter addresses the issue of retained austenite in quenched carburized steels. It explains why retained austenite can be expected at the surface of case-hardened components, how to estimate the amount that will be present, and how to effectively stabilize or otherwise control it. It presents detailed images and data plots showing how retained austenite appears and how it influences hardness, tensile properties, residual stresses, fatigue and fracture behaviors, and wear resistance.
Topics
Microsegregation,
Microstructure,
Inclusions,
Microcracking,
Gears,
Cold and cryogenic treatment,
Carburizing,
Case hardening,
Tempering,
Surface grinding,
Shot peening,
Roller burnishing,
Chemical composition,
Bending stress,
Hardenability,
Bending fatigue,
Rolling contact fatigue properties,
Wear resistance,
Core hardness,
Surface hardness,
Austenite,
Strain aging,
Quenching,
Alloy composition,
Carbon content,
Retained austenite
You do not currently have access to this chapter.
Citation
Retained Austenite, Carburizing: Microstructures and Properties, By Geoffrey Parrish, ASM International, 1999, p 77–97, https://doi.org/10.31399/asm.tb.cmp.t66770077
Download citation file:
Related Book Content
Carbides
Carburizing Microstructures and Properties
Postcarburizing Thermal Treatments
Carburizing Microstructures and Properties
Core Properties and Case Depth
Carburizing Microstructures and Properties
Postcarburizing Mechanical Treatments
Carburizing Microstructures and Properties
Decarburization
Carburizing Microstructures and Properties
Induction Hardening Gears
Heat Treatment of Gears A Practical Guide for Engineers
Induction and Flame Hardening
Gear Materials, Properties, and Manufacture
Internal Oxidation
Carburizing Microstructures and Properties
Hardenability Bands of Alloy Steels
Heat Treating of Irons and Steels
Failures of Shafts
Analysis and Prevention of Component and Equipment Failures