Aluminum Extrusion Technology
Chapter 4: Extrusion Die and Tooling
-
Published:2000
Abstract
This chapter familiarizes readers with the design, configuration, and function of tooling and dies used to extrude aluminum alloys. It discuses basic design considerations, including the geometry, location, and orientation of die openings; allowances for thermal shrinkage, stretching, and deflection; and the length and profile of bearing surfaces. It outlines the steps and processes involved in die making, describes the selection and treatment of die materials, and examines the factors that influence friction and wear. It also discusses the general procedures for on-site die correction.
Sign in
ASM members
Member Sign InExtrusion Die and Tooling, Aluminum Extrusion Technology, By Pradip K. Saha, ASM International, 2000, p 87–118, https://doi.org/10.31399/asm.tb.aet.t68260087
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!