Chapter 1: Fundamentals of Extrusion
-
Published:2000
Search within book:
Abstract
This chapter discusses the basic differences between direct and indirect extrusion, the application of plastic theory, the significance of strain and strain rate, friction, and pressure, and factors such as alloy flow stress and extrusion ratio, which influence the quality of material exiting the die and the amount of force required.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Fundamentals of Extrusion, Aluminum Extrusion Technology, By Pradip K. Saha, ASM International, 2000, p 1–29, https://doi.org/10.31399/asm.tb.aet.t68260001
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Die Wear
Metalworking: Bulk Forming
Machinery and Equipment for Direct and Indirect Hot Extrusion
Extrusion (Second Edition)
Extrusion Tooling
Extrusion (Second Edition)
Cold Extrusion of Aluminum Alloys
Aluminum Science and Technology
Extruded Products
Extrusion (Second Edition)
The Production of Extruded Semifinished Products from Metallic Materials
Extrusion (Second Edition)
Extrusion and Drawing of Aluminum Alloys
Aluminum Science and Technology
Fine-Edge Blanking
Metalworking: Sheet Forming
Conventional Hot Extrusion
Metalworking: Bulk Forming
Cold Extrusion
Metalworking: Bulk Forming