Book Chapter
Appendix 2: 400-Series PM Stainless Steels
-
Published:2007
Abstract
This appendix provides property data, including strength, tensile properties, elastic constants, and hardness, for 400-series powder metal stainless steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
400-Series PM Stainless Steels, Powder Metallurgy Stainless Steels: Processing, Microstructures, and Properties, By Erhard Klar, Prasan K. Samal, ASM International, 2007, p 221, https://doi.org/10.31399/asm.tb.pmsspmp.t52000221
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
300-Series PM Stainless Steels
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Brief Glossary of Terms
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Elastic Properties
Materials at Low Temperatures
Powder Metallurgy Processing by Hot Isostatic Pressing
Powder Metallurgy
Powder Metallurgy
Metals Fabrication Understanding the Basics
Powder Metallurgy
Titanium: A Technical Guide (Second Edition)
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Mechanical Properties Data for Selected Steels
Mechanics and Mechanisms of Fracture An Introduction
The Life of Harry Brearley (1871–1948)
The History of Stainless Steel
The Early Books and Papers on Stainless Steel (1917–1949)
The History of Stainless Steel