Abstract
Stainless steel powders are usually made by water or gas atomization. This chapter describes both processes and the properties and characteristics of the powders they produce. It also discusses secondary processes, including drying, screening, annealing, and lubricating, and the effects of iron contamination on corrosion resistance.
You do not currently have access to this chapter.
Citation
Manufacture and Characteristics of Stainless Steel Powders, Powder Metallurgy Stainless Steels: Processing, Microstructures, and Properties, By Erhard Klar, Prasan K. Samal, ASM International, 2007, p 23–38, https://doi.org/10.31399/asm.tb.pmsspmp.t52000023
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Manufacture of Stainless Steel Powders
Powder Metallurgy
Introduction to Metal Powder Production and Characterization
Powder Metallurgy
Powder Metallurgy Nickel and Nickel Alloys
Powder Metallurgy
Powder Metallurgy
Metals Fabrication Understanding the Basics
Introduction
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Production of Copper and Copper Alloy Powders
Powder Metallurgy
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Alloying Elements, Optimal Sintering, and Surface Modification in PM Stainless Steels
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Magnetic and Physical Properties
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Laser Powder Bed Fusion
Additive Manufacturing Processes