Abstract
This chapter recounts some of the early efforts and milestones in the development of stainless steel powders and their use in powder metallurgy applications.
Topics
Stainless steel powder
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Introduction, Powder Metallurgy Stainless Steels: Processing, Microstructures, and Properties, By Erhard Klar, Prasan K. Samal, ASM International, 2007, p 1–4, https://doi.org/10.31399/asm.tb.pmsspmp.t52000001
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Manufacture and Characteristics of Stainless Steel Powders
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Alloying Elements, Optimal Sintering, and Surface Modification in PM Stainless Steels
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Magnetic and Physical Properties
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Compacting and Shaping
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Powder Metallurgy Stainless Steels Applications
Powder Metallurgy