Appendix J: Dislocation Etching Techniques
-
Published:1984
Abstract
This appendix is a list of etchants that are used to reveal dislocations in various metals, alloys, and compounds.
This content is PDF only. Please click on the PDF icon to access.
You do not currently have access to this chapter.
Citation
Dislocation Etching Techniques, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 712–731, https://doi.org/10.31399/asm.tb.mpp.t67850712
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Etchants for Revealing Microstructure
Metallography Principles and Practice
Etching Methods
Light Microscopy of Carbon Steels
Metallographic Technique: Micrography
Metallography of Steels Interpretation of Structure and the Effects of Processing
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Attack Polishing Procedures
Metallography Principles and Practice
Chemical Polishing Solutions
Metallography Principles and Practice
Description of Hardness Code and Specification of Hardness Numbers for Metals
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Metric Conversions
Elements of Metallurgy and Engineering Alloys