Abstract
This appendix contains recipes of the electrolytic solutions in which various metals are polished in preparation for metallographic examination.
Topics
Grain structure,
Macrostructure,
Microstructure,
Inclusions,
Quantitative fractography,
Polishing machines,
Dynamic hardness testing,
Indentation hardness testing,
Metallography,
Optical light microscopy,
Photomacrography,
Photomicrography,
Polishing,
Ferrous metals and alloys,
Nonferrous metals and alloys,
Optical microscopes,
Specimen preparation
This content is PDF only. Please click on the PDF icon to access.
You do not currently have access to this chapter.
Citation
Electromechanical Polishing Procedures, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 541–542, https://doi.org/10.31399/asm.tb.mpp.t67850541
Download citation file:
Related Book Content
Electrolytic Polishing Solutions
Metallography Principles and Practice
Chemical and Electrolytic Polishing
Metallography and Microstructures
Electropolishing
Corrosion: Fundamentals, Testing, and Protection
Electrochemical Machining
Corrosion: Fundamentals, Testing, and Protection
Mechanical Grinding and Polishing
Metallography and Microstructures
Corrosion in Bridges and Highways
Corrosion: Environments and Industries