This appendix provides a list of etch compositions and procedures that reveal the macrostructure of aluminum, beryllium, bismuth, antimony, cobalt, copper, lead, magnesium, nickel, tin, titanium, zinc, and their respective alloys as well as iron, steel, noble metals, refractory metals, silicon, zirconium, and hafnium.
You do not currently have access to this chapter.
Citation
Etchants for Revealing Macrostructure, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 509–532, https://doi.org/10.31399/asm.tb.mpp.t67850509
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Macroetchants for Revealing Strain Patterns in Nonferrous Metals
Metallography Principles and Practice
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Attack Polishing Procedures
Metallography Principles and Practice
Chemical Polishing Solutions
Metallography Principles and Practice
Description of Hardness Code and Specification of Hardness Numbers for Metals
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Electrolytic Polishing Solutions
Metallography Principles and Practice
Dislocation Etching Techniques
Metallography Principles and Practice
Corrosion Rate Conversion
Corrosion in the Petrochemical Industry (Second Edition)