Chapter 6: Quantitative Microscopy
-
Published:1984
Abstract
This chapter covers the emerging practice of quantitative microscopy and its application in the study of the microstructure of metals. It describes the methods used to quantify structural gradients, volume fraction, grain size and distribution, and other features of interest. It provides examples showing how the various features appear, how they are measured, and how the resulting data are converted into usable form. The chapter also discusses the quantification of fracture morphology and its correlation with material properties and behaviors.
Topics
Grain structure,
Macrostructure,
Microstructure,
Inclusions,
Quantitative fractography,
Polishing machines,
Dynamic hardness testing,
Indentation hardness testing,
Metallography,
Optical light microscopy,
Photomacrography,
Photomicrography,
Polishing,
Ferrous metals and alloys,
Nonferrous metals and alloys,
Optical microscopes,
Grain morphology,
Microstructural analysis,
Electron microscopy
You do not currently have access to this chapter.
Citation
Quantitative Microscopy, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 410–508, https://doi.org/10.31399/asm.tb.mpp.t67850410
Download citation file:
Related Book Content
Cast Aluminum-Silicon Alloy—Phase Constituents and Microstructure
Aluminum-Silicon Casting Alloys Atlas of Microstructures
Fractal Analysis of Fracture Surfaces
Fractography
Quantitative Fractography
Failure Analysis and Prevention
Quantitative Fractography
Fractography
Advanced Techniques of Failure Analysis
Failure Analysis of Engineering Structures Methodology and Case Histories
History of Fractography
Fractography
Metallography of Titanium and Its Alloys
Titanium Physical Metallurgy, Processing, and Applications
Modeling of Dendritic Grain Solidification
Metals Process Simulation
Measurement of Microstructure
Metals Handbook Desk Edition (2nd Edition)
Failure of a Fuel Nozzle in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories