This chapter explains how to achieve accurate, sharp delineation of the microstructure of metals using appropriate etching and contrasting techniques. It covers a variety of methods, including chemical etching, heat tinting, gas contrasting, vapor deposition, magnetic etching, ion bombardment, and dislocation etch pitting.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Microstructure, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 165–266, https://doi.org/10.31399/asm.tb.mpp.t67850165
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Visual Identification of Microstructural Constituents in Metallographic Cross Sections
Aluminum-Silicon Casting Alloys Atlas of Microstructures
The Art of Revealing Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Etching Methods
Light Microscopy of Carbon Steels
Metallography and Microstructures of Lead and Its Alloys
Metallography and Microstructures
Metallography and Microstructures of Case-Hardening Steel
Metallography and Microstructures
Metallography and Microstructures of Low-Carbon and Coated Steels
Metallography and Microstructures
Metallographic Technique: Macrography
Metallography of Steels Interpretation of Structure and the Effects of Processing
Metallography and Microstructures of Zirconium, Hafnium, and Their Alloys
Metallography and Microstructures
Etching of Aluminum and Its Alloys
Aluminum Science and Technology
Metallographic Technique: Micrography
Metallography of Steels Interpretation of Structure and the Effects of Processing