Chapter 2: Specimen Preparation for Light Microscopy
-
Published:1984
Abstract
This chapter explains how to prepare metallographic samples for light microscopy and how to anticipate and avoid related problems. It describes standard practices and procedures for sectioning, mounting, grinding, and polishing and identifies common defects along with their causes and cures. It also provides recommendations for handling specific materials and addresses safety concerns.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Specimen Preparation for Light Microscopy, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 60–164, https://doi.org/10.31399/asm.tb.mpp.t67850060
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Optical Metallography
Materials Characterization
Microstructural Characterization of Thermal Spray Coatings
Metallography and Microstructures
Introduction
Light Microscopy of Carbon Steels
Glossary of Terms
Light Microscopy of Carbon Steels
Metallographic Sectioning and Specimen Extraction
Metallography and Microstructures
Tempering of Martensite
Light Microscopy of Carbon Steels
Light Microscopy
Metallography Principles and Practice
Principles and Procedures of Fractography
Metals Handbook Desk Edition (2nd Edition)
Light and Electron Microscopy
Metallography and Microstructures
Scanning Electron Microscopy
Fractography