Chapter 1: Macrostructure
-
Published:1984
Abstract
This chapter describes several macroscopic examination techniques, including macroetching, contact printing, fracturing, and lead exudation. It explains how each method is implemented, why it is used, and what it reveals about manufacturing processes, defects, imperfections, and failure mechanisms.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Macrostructure, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 1–59, https://doi.org/10.31399/asm.tb.mpp.t67850001
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Failure of an LP Turbine Disc in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Glossary of Terms, Symbols, and Abbreviations
Mechanics and Mechanisms of Fracture An Introduction
Macroetching
Metallography and Microstructures
Quality Control
Practical Induction Heat Treating (Second Edition)
Metallography and Microstructures of Magnesium and Its Alloys
Metallography and Microstructures
Fracture Analysis
Cast Iron Science and Technology
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Quality Management in Extrusion
Extrusion (Second Edition)
Sensors for Sheet Metal Forming
Sheet Metal Forming Processes and Applications