Chapter 12: Relationships among Structures, Processing, and Properties
-
Published:2000
Abstract
This chapter examines the process, structure, and property relationships in titanium alloys. It provides information on microstructures and strengthening mechanisms, the role of alloy and interstitial elements, and the effect of composition, processing, and surface treatments on tensile and yield strength, fracture toughness, hardness, ductility, and creep and fatigue behaviors. The chapter covers wrought, cast, and powder metal titanium alloys and contains an extensive amount of property data.
Sign in
ASM members
Member Sign InRelationships among Structures, Processing, and Properties, Titanium: A Technical Guide, 2nd ed., By Matthew J. Donachie, Jr., ASM International, 2000, p 95–121, https://doi.org/10.31399/asm.tb.ttg2.t61120095
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.