Chapter 11: Cleaning and Finishing
-
Published:2000
Abstract
Cleaning procedures serve to remove scale, tarnish films, and other contaminants that form or are otherwise deposited on the surface of titanium during processing operations such as hot working and heat treatment. This chapter explains what makes titanium susceptible to the formation of scale and how it can be removed via belt grinding, abrasive blasting, and molten salt descaling baths. It also discusses the role of acid pickling, barrel finishing, polishing, and buffing as well as the use of chemical conversion coatings and protective platings.
Topics
Microstructure,
Corrosion,
Cast product forms,
Titanium powder,
Wrought product forms,
Titanium alloys,
Casting,
Conversion coating,
Plating,
Heat treatment,
Welding,
Machining,
Forging,
Forming,
Powder metallurgy,
Surface treatment,
Alloy composition,
Machinability,
Mechanical properties,
Physical properties,
Materials selection,
Titanium-matrix composites,
Phase diagrams,
Time-temperature transformation diagram,
Chemical conversion coatings,
Electroplating,
Cleaning,
Barrel finishing
You do not currently have access to this chapter.
Citation
Cleaning and Finishing, Titanium: A Technical Guide, 2nd ed., By Matthew J. Donachie, Jr., ASM International, 2000, p 85–93, https://doi.org/10.31399/asm.tb.ttg2.t61120085
Download citation file:
Related Book Content
Surface Engineering of Aluminum and Aluminum Alloys
Surface Engineering
Surface Engineering of Titanium and Titanium Alloys
Surface Engineering
Surface Engineering of Heat-Resistant Alloys
Surface Engineering
Chemical Conversion Coatings
Aluminum Science and Technology
Cleaning and Rust Protection
Practical Induction Heat Treating (Second Edition)
Dip, Barrier, and Chemical Conversion Coatings
Metals Handbook Desk Edition (2nd Edition)
Summary Table of Titanium Alloys
Titanium: A Technical Guide (Second Edition)
Titanium Alloy Datasheets Introduction
Titanium: A Technical Guide (Second Edition)
Cross Reference to Equivalent Titanium Alloys
Titanium: A Technical Guide (Second Edition)
Finishing and Coating
Metals Fabrication Understanding the Basics