Abstract
This chapter describes the applications with the greatest impact on titanium consumption and global market trends. It explains where, how, and why titanium alloys are used in aerospace, automotive, chemical processing, medical, and military applications as well as power generating equipment, sporting goods, oil and gas production, and marine vessels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Applications of Titanium, Titanium: Physical Metallurgy, Processing, and Applications, Edited By F.H. Froes, ASM International, 2015, p 353–380, https://doi.org/10.31399/asm.tb.tpmpa.t54480353
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Properties, Compositions, and Applications of Selected Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Applications for Metal Powder Injection Molding
Powder Metallurgy
Tantalum
Materials for Medical Devices
A Primer on Titanium and Its Alloys
Titanium: A Technical Guide (Second Edition)
Selected Manufacturers, Suppliers, Services
Titanium: A Technical Guide (Second Edition)
Symbols
Titanium: A Technical Guide (Second Edition)
Glossary
Titanium: A Technical Guide (Second Edition)
Selected References for Additional Reading
Titanium: A Technical Guide (Second Edition)
Listing of Selected Specification and Standardization Organizations
Titanium: A Technical Guide (Second Edition)
Aluminum—The Light Metal
The History of Metals in America