Titanium: Physical Metallurgy, Processing, and Applications
Abstract
This chapter familiarizes readers with the machining characteristics of titanium and the implementation of machining and shaping processes. It explains why titanium alloys are more difficult to machine than other metals and how it impacts the equipment and procedures that can be used. It describes the basic machining requirements for titanium in terms of tool geometry and materials, machine setup rigidity, cutting speeds and feed rates, and surface conditions, and explains how the requirements are met in practice in milling, turning, drilling, surface grinding, and broaching operations. The chapter also covers chemical and electrochemical machining processes as well as...
Sign in
ASM members
Member Sign InMachining and Chemical Shaping of Titanium, Titanium: Physical Metallurgy, Processing, and Applications, Edited By F.H. Froes, ASM International, 2015, p 293–329, https://doi.org/10.31399/asm.tb.tpmpa.t54480293
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.