Most integrated titanium mills have primary working equipment designed specifically for titanium. This chapter describes the forging, rolling, and extruding equipment used to produce titanium mill products and sheds light on the corresponding process, structure, property relationships.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Primary Working, Titanium: Physical Metallurgy, Processing, and Applications, Edited By F.H. Froes, ASM International, 2015, p 207–223, https://doi.org/10.31399/asm.tb.tpmpa.t54480207
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Glossary: Bulk Forming
Metalworking: Bulk Forming
Metalworking
Beryllium Chemistry and Processing
Deformation Processing
Elements of Metallurgy and Engineering Alloys
Bulk Deformation
Metals Fabrication Understanding the Basics
Secondary Working of Bar and Billet
Titanium Physical Metallurgy, Processing, and Applications
Corrosion Resistance of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Beryllium and Aluminum-Beryllium Alloys
Powder Metallurgy
Cold Welding
Welding Fundamentals and Processes
Primary Mill Fabrication
Metals Fabrication Understanding the Basics
Research and Development
Aluminum Extrusion Technology