Titanium: Physical Metallurgy, Processing, and Applications
Abstract
The practical application of metals and alloys is guided largely by information obtained through the study of their microstructure. This chapter examines a wide range of titanium microstructures, identifying characteristic features and explaining what they reveal about processing, properties, and performance. It includes images of elongated and equiaxed structures, primary alpha, transformed beta, and metastable phases as well as spheroidal and intergranular beta, alpha case, and intermetallic compounds. It also defines important terms and provides step-by-step procedures for preparing titanium for metallographic analysis.
Sign in
ASM members
Member Sign InMetallography of Titanium and Its Alloys, Titanium: Physical Metallurgy, Processing, and Applications, Edited By F.H. Froes, ASM International, 2015, p 141–159, https://doi.org/10.31399/asm.tb.tpmpa.t54480141
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.