Structural Composite Materials
Chapter 21: Ceramic Matrix Composites
-
Published:2010
Abstract
This chapter discusses the types of fibers and matrix materials used in ceramic matrix composites and the role of interfacial coatings. It describes the methods used to produce ceramic composites, including powder processing, slurry infiltration and consolidation, polymer infiltration and pyrolysis, chemical vapor infiltration, directed metal oxidation, and liquid silicon infiltration.
Sign in
ASM members
Member Sign InCeramic Matrix Composites, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 573–596, https://doi.org/10.31399/asm.tb.scm.t52870573