Chapter 13: Mechanical Property Test Methods
-
Published:2010
Abstract
This chapter discusses composite testing procedures, including tension, compression, shear, flexure, and fracture toughness testing as well as adhesive shear, peel, and honeycomb flatwise tension testing. It also discusses specimen preparation, environmental conditioning, and data analysis.
Topics
Environmental degradation,
Adhesion testing,
Composites products and forms,
Composite processing,
Adhesive bonding,
Mechanical fastening,
Nondestructive testing,
Materials selection,
Structural analysis,
Ceramic-matrix composites,
Sandwich structures,
Ceramic matrices,
Metallic matrices,
Organic matrices,
Aluminum-matrix composites,
Titanium-matrix composites,
Polymer-matrix composites,
Fibers,
Fiber-reinforced composites,
Peel testing,
Fracture toughness testing,
Composites,
Shear testing,
Tensile testing,
Specimen preparation
You do not currently have access to this chapter.
Citation
Mechanical Property Test Methods, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 351–372, https://doi.org/10.31399/asm.tb.scm.t52870351
Download citation file:
Related Book Content
Ultrasonic Additive Manufacturing
Additive Manufacturing Processes
Mechanical Testing
Metals Handbook Desk Edition (2nd Edition)
Mechanical Testing of Fiber-Reinforced Composites
Mechanical Testing and Evaluation
X-Ray Diffraction Residual Stress Measurement in Failure Analysis
Failure Analysis and Prevention
Shear, Torsion, and Multiaxial Testing
Mechanical Testing and Evaluation
Repair
Structural Composite Materials
Glossary of Filament-Winding Terms
Composite Filament Winding
Tension and Compression Testing at Low Temperatures
Mechanical Testing and Evaluation
Out-of-Plane Analysis
Composites