Chapter 6: Thermoplastic Composite Fabrication Processes
-
Published:2010
Abstract
This chapter discusses thermoplastic composite fabrication processes and related equipment and procedures. The discussion covers consolidation and thermoforming operations as well as joining methods.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Thermoplastic Composite Fabrication Processes, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 183–200, https://doi.org/10.31399/asm.tb.scm.t52870183
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Hot Isostatic Pressing for Metal Additive Manufacturing
Additive Manufacturing Processes
Fabrication Tooling
Structural Composite Materials
Introduction to Constituent Materials
Composites
Thermoforming
Engineered Materials Handbook Desk Edition
Joining of Organic-Matrix Composites
Welding, Brazing, and Soldering
Engineering Plastics
Lightweight Materials Understanding the Basics
Thermoplastic Composites Manufacturing
Composites
Introduction to Special Welding and Joining Topics
Welding, Brazing, and Soldering
Design for Plastics Processing
Materials Selection and Design