Abstract
This appendix discusses the sizing, scaling, and configuration requirements of the basic components in a quench cooling system, including tanks, pumps, hoses, and inlet and outlet fixtures and the materials from which they are made.
Topics
Quenching
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Quench System Design, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 335–341, https://doi.org/10.31399/asm.tb.piht2.t55050335
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.