Chapter 12: Standards and Inspection
-
Published:2015
Abstract
This chapter discusses the methods and procedures used for inspecting induction-hardened parts. It provides information on hardness and case depth measurements, nondestructive testing and surface analysis, the effect of various hardening errors, and relevant test standards.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Standards and Inspection, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 245–262, https://doi.org/10.31399/asm.tb.piht2.t55050245
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Principles of Induction Hardening and Inspection
Induction Heating and Heat Treatment
Inspection and NDT Methods
Induction Heating and Heat Treatment
Testing and Inspection of Metals—The Quest for Quality
Metallurgy for the Non-Metallurgist (Second Edition)
Induction Case Hardening of Axle Shafts
Induction Heating and Heat Treatment
Inspection Methods: Overview and Comparison
Inspection of Metals Understanding the Basics
Postcoating Operations
Thermal Spray Technology
Induction Hardening of Gears and Gear-Like Components
Induction Heating and Heat Treatment
Carbonitriding of Steels
Steel Heat Treating Fundamentals and Processes
Cracked Aircraft Wing Spar
ASM Failure Analysis Case Histories: Air and Spacecraft
Defects and Abnormal Characteristics of Induction Hardened Components
Induction Heating and Heat Treatment