Book Chapter
Chapter 6: Quenching
-
Published:2015
Abstract
This chapter discusses the quenching process and its adaptation to induction heat treating. It describes the three stages of quenching, the cooling characteristics of various types of quenchants, and the details of nearly a dozen compatible quenching methods. It also explains how to verify whether a quenchant can cool a workpiece fast enough to achieve martensitic transformation without cracking or distortion.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Quenching, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 139–154, https://doi.org/10.31399/asm.tb.piht2.t55050139
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Quenching with Molten Metal
Steel Heat Treating Technologies
Quenchant Agitation, Design, and Characterization
Steel Heat Treating Technologies
Quench Factor Characterization of Quenchants for Hardening of Steel
Steel Heat Treating Technologies
Transformation of Austenite and Quenching of Steel
Practical Heat Treating Basic Principles
Design and Fabrication of Inductors for Induction Heat Treating
Induction Heating and Heat Treatment
Metallurgical Definitions for Induction Heat Treating
Practical Induction Heat Treating (Second Edition)
Quenching of Induction Heated Steel
Induction Heating and Heat Treatment
Induction Heat Treating Systems
Practical Induction Heat Treating (Second Edition)
Nonconforming Product and Process Problems
Practical Induction Heat Treating (Second Edition)
Quenchants Used for Heat Treatment of Ferrous Alloys
Steel Heat Treating Technologies