Practical Induction Heat Treating (Second Edition)
Chapter 2: Theory of Heating by Induction
-
Published:2015
Abstract
This chapter discusses the basic principles of induction heating and related engineering considerations. It describes the design and operation of induction coils, the magnitude and distribution of magnetic fields, and the forces that generate eddy currents in metals. It explains how induced electrical current causes metal to heat in proportion to their electrical resistance and how it affects temperature dependent properties such as resistivity and specific heat and, in turn, heating rates and efficiencies. It also discusses the effect of hysteresis and explains why eddy currents tend to be confined to the outer surface of the workpiece, a phenomenon...
Sign in
ASM members
Member Sign InTheory of Heating by Induction, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 9–23, https://doi.org/10.31399/asm.tb.piht2.t55050009
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.