Practical Heat Treating: Basic Principles
Chapter 12: Heat Treatment of Aluminum and Other Nonferrous Alloys
-
Published:2020
Abstract
The term heat treatable alloys is used in reference to alloys that can be hardened by heat treatment, and this chapter briefly describes the major types of heat treatable nonferrous alloys. The discussion provides a general description of annealing cold-worked metals and describes some of the common nonferrous alloys that can be hardened through heat treatment. The nonferrous alloys covered include aluminum alloys, cobalt alloys, copper alloys, magnesium alloys, nickel alloys, and titanium alloys.
Sign in
ASM members
Member Sign InHeat Treatment of Aluminum and Other Nonferrous Alloys, Practical Heat Treating: Basic Principles, By Jon L. Dossett, ASM International, 2020, p 351–386, https://doi.org/10.31399/asm.tb.phtbp.t59310351
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.