Chapter 7: Hardening and Tempering of Steel
-
Published:2020
Abstract
This chapter discusses the processes involved in the heat treatment of steel, namely austenitizing, hardening, quenching, and tempering. It begins with an overview of austenitizing of steels by induction heating, followed by a discussion on the processes involved in transformation of the soft austenite into martensite or lower bainite in the hardening operation. The chapter provides information on various quenching systems and a description of quenching techniques, namely austempering, martempering, and patenting. Difficulties associated with hardening of steel are discussed. Further, the chapter describes the equipment used for and principal variables of tempering. It discusses the causes for various...
Sign in
ASM members
Member Sign InHardening and Tempering of Steel, Practical Heat Treating: Basic Principles, By Jon L. Dossett, ASM International, 2020, p 163–201, https://doi.org/10.31399/asm.tb.phtbp.t59310163
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!