Surface Engineering for Corrosion and Wear Resistance
Chapter 6: Surface Engineering to Add a Surface Layer or Coating
-
Published:2001
Abstract
This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld overlays, thermal spraying, and various deposition technologies.