Surface Engineering for Corrosion and Wear Resistance
Chapter 1: Introduction to Surface Engineering for Corrosion and Wear Resistance
-
Published:2001
Abstract
This chapter begins with a brief review of the different types of surface treatments and coatings used in industry and their effect on properties and performance. It then discusses the importance of corrosion and wear treatments and the consequences of failing to properly implement them in critical industries such as mining, energy production, transportation, and mineral and chemical processing. The chapter also describes basic approaches to dealing with corrosion and wear in steel.
Sign in
ASM members
Member Sign InIntroduction to Surface Engineering for Corrosion and Wear Resistance, Surface Engineering for Corrosion and Wear Resistance, Edited By J.R. Davis, ASM International, 2001, p 1–10, https://doi.org/10.31399/asm.tb.secwr.t68350001
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.