Appendix 10: Mechanical Properties Data for Selected Steels
-
Published:2005
Abstract
This appendix provides tensile property and fracture toughness data for various low-alloy and stainless steels.
Topics
Stacking faults,
Twinning,
Damage tolerance assessment,
Crack initiation,
Crack propagation,
Creep deformation,
Mixed-mode fracture,
Fractography,
Steel,
Aluminum alloys,
Titanium alloys,
Ceramics,
Glasses,
Polymers,
Finite element analysis,
Mechanical properties,
Elastic-plastic fracture toughness,
Plane strain fracture toughness,
Stress-strain curves,
Stress analysis,
Polymer-matrix composites,
Stainless steel,
Low-alloy steel,
Fracture toughness,
Tensile properties
You do not currently have access to this chapter.
Citation
Mechanical Properties Data for Selected Steels, Mechanics and Mechanisms of Fracture: An Introduction, By Alan F. Liu, ASM International, 2005, p 423–427, https://doi.org/10.31399/asm.tb.mmfi.t69540423
Download citation file:
Related Book Content
Dissimilar Welds With Stainless Steels
Welding, Brazing, and Soldering
Shielded Metal Arc Welding
Welding, Brazing, and Soldering
Dip Brazing
Welding, Brazing, and Soldering
Dilution in Fusion Welding
Welding Fundamentals and Processes
The Art of Revealing Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Corrosion of Containment Materials for Radioactive-Waste Isolation
Corrosion: Environments and Industries
Austenitizing Temperatures for Steels
Failure Analysis of Heat Treated Steel Components
Stress-Corrosion Cracking of Carbon and Low-Alloy Steels (Yield Strengths Less Than 1241 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Glossary of Selected Terms
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Properties of Carbon Alloy Steel Welds
Weld Integrity and Performance