Appendix 10: Mechanical Properties Data for Selected Steels
-
Published:2005
Search within book:
Abstract
This appendix provides tensile property and fracture toughness data for various low-alloy and stainless steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Mechanical Properties Data for Selected Steels, Mechanics and Mechanisms of Fracture: An Introduction, By Alan F. Liu, ASM International, 2005, p 423–427, https://doi.org/10.31399/asm.tb.mmfi.t69540423
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Dissimilar Welds With Stainless Steels
Welding, Brazing, and Soldering
Shielded Metal Arc Welding
Welding, Brazing, and Soldering
Dip Brazing
Welding, Brazing, and Soldering
Dilution in Fusion Welding
Welding Fundamentals and Processes
The Art of Revealing Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Corrosion of Containment Materials for Radioactive-Waste Isolation
Corrosion: Environments and Industries
Stress-Corrosion Cracking of Carbon and Low-Alloy Steels (Yield Strengths Less Than 1241 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Austenitizing Temperatures for Steels
Failure Analysis of Heat Treated Steel Components
Glossary of Selected Terms
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
AISI to Non-AISI Steel Cross Reference
Failure Analysis of Heat Treated Steel Components