Abstract
This chapter describes the factors that affect the corrosion performance of aluminum assemblies joined by methods such as welding, brazing, soldering, and adhesive bonding. The factors covered include galvanic effects, crevices, and assembly stresses in products susceptible to stress-corrosion cracking.
Topics
Aqueous corrosion,
Atmospheric corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Erosion corrosion,
Galvanic corrosion,
Intergranular corrosion,
Weld corrosion,
Stray current corrosion,
Corrosion fatigue,
Stress corrosion cracking,
Corrosion inhibitors,
Cast aluminum alloys,
Wrought aluminum alloys,
Aluminum alloys,
Anodizing,
Cladding,
Chromate conversion coating,
Plating,
Cleaning,
Alloy composition,
Corrosion testing,
Aluminum-matrix composites,
Corrosion,
Adhesive bonding,
Brazing,
Soldering,
Welding,
Aluminum
You do not currently have access to this chapter.
Citation
Corrosion of Welded, Brazed, Soldered, and Adhesive-Bonded Joints, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 161–178, https://doi.org/10.31399/asm.tb.caaa.t67870161
Download citation file:
Related Book Content
An Overview of Joining Processes
Welding Fundamentals and Processes
Design for Joining
Materials Selection and Design
Introduction and Overview of Joining
Metals Handbook Desk Edition (2nd Edition)
Introduction to Special Welding and Joining Topics
Welding, Brazing, and Soldering
Welding and Joining of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Introduction to Brazing and Soldering
Welding, Brazing, and Soldering
Materials Issues in Joining
Joining Understanding the Basics
Corrosion of Dissimilar Metal Weldments
Corrosion of Weldments
Introduction to Joining
Joining Understanding the Basics
Overview of Welding Processes
Welding Fundamentals and Processes