Abstract
This chapter discusses three related corrosion mechanisms, galvanic, deposition, and stray-current corrosion, explaining why they occur and how they affect the corrosion process. It includes information on testing and prevention methods along with examples of the type of damage associated with these corrosion mechanisms.
You do not currently have access to this chapter.
Citation
Galvanic, Deposition, and Stray-Current Corrosion, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 75–83, https://doi.org/10.31399/asm.tb.caaa.t67870075
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Stray-Current Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Pitting and Crevice Corrosion
Corrosion of Aluminum and Aluminum Alloys
Corrosion of Aluminum and Aluminum Alloys
Corrosion: Materials
External Corrosion of Oil and Natural Gas Pipelines
Corrosion in the Petrochemical Industry (Second Edition)
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
U.S. Navy Aircraft Corrosion
Corrosion: Environments and Industries
Failure of Aluminum Alloy Spacers by Galvanic Attack
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology