Abstract
This chapter discusses three related corrosion mechanisms, galvanic, deposition, and stray-current corrosion, explaining why they occur and how they affect the corrosion process. It includes information on testing and prevention methods along with examples of the type of damage associated with these corrosion mechanisms.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Galvanic, Deposition, and Stray-Current Corrosion, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 75–83, https://doi.org/10.31399/asm.tb.caaa.t67870075
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Stray-Current Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Pitting and Crevice Corrosion
Corrosion of Aluminum and Aluminum Alloys
Corrosion of Aluminum and Aluminum Alloys
Corrosion: Materials
External Corrosion of Oil and Natural Gas Pipelines
Corrosion in the Petrochemical Industry (Second Edition)
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
U.S. Navy Aircraft Corrosion
Corrosion: Environments and Industries
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology
Aluminum—The Light Metal
The History of Metals in America