This chapter discusses some of the methods and measurements used to construct phase diagrams. It explains how cooling curves were widely used to determine phase boundaries, and how equilibrated alloys examined under controlled heating and cooling provide information for constructing isothermal and vertical sections as well as liquid projections. It also explains how diffusion couples provide a window into local equilibria and identifies typical phase diagram construction errors along with problems stemming from phase-boundary curvatures and congruent transformations.
Sign in
ASM members
Member Sign InPhase Diagram Determination, Phase Diagrams: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 239–262, https://doi.org/10.31399/asm.tb.pdub.t53420239
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.