This chapter explains how the presence of intermediate phases affects the melting behavior of binary alloys and the transformations that occur under different rates of cooling. It begins by examining the phase diagrams of magnesium-lead and copper-zinc, noting some of the complexities associated with intermediate phases. It then discusses the difference between ordered and disordered phases and how they are accounted for on phase diagrams. It describes how the atoms in a disordered solution may arrange themselves into an ordered array, forming a superlattice in the process of cooling, and goes on to identify the most common superlattice structures...