Phase Diagrams: Understanding the Basics
Edited by
ASM International
ISBN electronic:
978-1-62708-310-2
Publication date:
2012
Book Chapter
Chapter 6: Peritectic Alloy Systems
-
Published:2012
Abstract
This chapter discusses the phase transformations of peritectic alloy systems. It describes the processes involved with equilibrium and nonequilibrium freezing, the mechanisms of peritectic formation, and the resulting microstructures. It also discusses the formation of peritectic structures in iron-base alloys and multicomponent systems.
You do not currently have access to this chapter.
Citation
Peritectic Alloy Systems, Phase Diagrams: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 117–134, https://doi.org/10.31399/asm.tb.pdub.t53420117
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Peritectic Alloy Systems
Alloy Phase Diagrams
Peritectic Solidification
Casting
Glossary of Terms: Metallography and Microstructure
Metallography and Microstructures
Abbreviations and Symbols: Metallography and Microstructure
Metallography and Microstructures
Ductile Fracture
Understanding How Components Fail (Third Edition)
Microstructure
Metallography Principles and Practice
Failure and Refurbishment
Superalloys: A Technical Guide (Second Edition)
Tempering of Steel
Steels: Processing, Structure, and Performance (Second Edition)
Spinodal Transformation Structures
Metallography and Microstructures
Micrograph Gallery
Superalloys Alloying and Performance