Book Chapter
Chapter 1: Introduction to Phase Diagrams
-
Published:2012
Abstract
This chapter provides a brief overview of phase diagrams, explaining what they represent and how and why they are used. It identifies key points, lines, and features on a binary nickel-copper phase diagram and explains what they mean from a practical perspective. It also discusses the concept of equilibrium, the significance of Gibb’s phase rule, the theorem of Le Chatelier, and the use of the lever rule.
Topics
Transformation temperature,
Crystal structure,
Deformation structures,
Solidification structures,
Solid-state transformation structures,
Precipitation hardening,
Tempering,
CALPHAD method,
Chemical potential,
Phase transformation properties,
Phase transition temperatures,
Alloy systems,
Phase diagrams,
Time-temperature transformation diagram,
Liquid,
Solid,
Isothermal transformation,
Solidification,
Binary phase diagram,
Phase equilibria
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Introduction to Phase Diagrams, Phase Diagrams: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 1–13, https://doi.org/10.31399/asm.tb.pdub.t53420001
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Beryllium Binary Phase Diagrams
Beryllium Chemistry and Processing
Introduction to Phase Diagrams
Alloy Phase Diagrams
Intermediate Phases
Alloy Phase Diagrams
Isomorphous Alloy Systems
Alloy Phase Diagrams