Chapter 12: Selection Guidelines for Lightweight Materials
-
Published:2012
Abstract
This chapter consists of three parts. The first part provides data and guidelines for selecting materials and processing routes. It compares the basic properties of metals, ceramics, and polymers, identifies important measures of performance, and discusses manufacturing processes and their compatibility with specific materials. The chapter then presents general guidelines for selecting lightweight materials, and concludes with a review of lightweight metals, plastics, and composites used in automotive applications.
Topics
Corrosion,
Wrought product forms,
Polymer product forms,
Aluminum alloys,
Beryllium alloys,
Magnesium alloys,
Titanium alloys,
Thermoplastics,
Thermosetting plastics,
Casting,
Joining,
Machining,
Forging,
Forming,
Mechanical properties,
Physical properties,
Materials selection,
Ceramic-matrix composites,
Titanium-aluminide composites,
Metal-matrix composites,
Polymer-matrix composites,
Automotive materials
You do not currently have access to this chapter.
Citation
Selection Guidelines for Lightweight Materials, Lightweight Materials: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 621–672, https://doi.org/10.31399/asm.tb.lmub.t53550621
Download citation file:
Related Book Content
Introduction and Uses of Lightweight Materials
Lightweight Materials Understanding the Basics
Introduction to Selection of Titanium Alloys
Titanium: A Technical Guide (Second Edition)
Some Considerations in the Selection of a Superalloy
Superalloys Alloying and Performance
Designing to Minimize Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Materials Selection for Failure Prevention
Failure Analysis and Prevention
Design and Certification Considerations
Structural Composite Materials
Materials Selection for Failure Prevention
Analysis and Prevention of Component and Equipment Failures
Avoiding Plastic Product Failure by Proper Plastic Selection and Design
Characterization and Failure Analysis of Plastics
Laser Weld Quality Monitoring
Welding Fundamentals and Processes