Chapter 10: Coal-Fired Boilers
-
Published:2007
Abstract
This chapter discusses material-related problems associated with coal-fired burners. It explains how high temperatures affect heat-absorbing surfaces in furnace combustion areas and in the convection pass of superheaters and reheaters. It describes how low-NOx combustion technology, intended to reduce NOx emissions, accelerates tube wall wastage. It also covers circumferential cracking in furnace waterwalls, thermal fatigue cracking induced by waterlances and water cannons, superheater-reheater corrosion, and erosion in fluidized-bed boilers.
Topics
Stress-induced corrosion,
High-temperature corrosion,
Erosion corrosion,
Stress corrosion cracking,
Liquid metal embrittlement,
Steel,
Boilers,
Incinerators and incineration equipment,
Waste-heat recovery systems,
Fuel-fired furnaces,
Recovery boilers,
Liquor processing and handling equipment,
Fireside corrosion,
Coal-fired boilers,
Combustion furnaces,
Thermal fatigue fracture
You do not currently have access to this chapter.
Citation
Coal-Fired Boilers, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 259–320, https://doi.org/10.31399/asm.tb.htcma.t52080259
Download citation file:
Related Book Content
Hydrogen Attack
High-Temperature Corrosion and Materials Applications
Erosion and Erosion-Corrosion
High-Temperature Corrosion and Materials Applications
Corrosion Failures in Gas Turbine Hot Components
Handbook of Case Histories in Failure Analysis
Corrosion Control by Proper Design
Corrosion: Understanding the Basics
Erosive Wear Failures
Failure Analysis and Prevention (2021 Edition)
Wear Failures
Fatigue and Fracture Understanding the Basics
Corrosion Resistance of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Corrosion of Titanium and Titanium Alloys
Corrosion: Materials
Materials Selection for Corrosion Control
Corrosion in the Petrochemical Industry (Second Edition)
Forms of Corrosion: Recognition and Prevention
Corrosion: Understanding the Basics