Abstract
This chapter explains how materials selection becomes much more difficult when designing for high-temperature corrosion environments. It also discusses the use of cladding and weld overlays to compensate for material deficiencies and prolong service life.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Challenges in Materials Applications for High-Temperature Service, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 3–4, https://doi.org/10.31399/asm.tb.htcma.t52080003
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Introduction
High-Temperature Corrosion and Materials Applications
Registered Trademarks and Trademarks
High-Temperature Corrosion and Materials Applications
Corrosion by Halogen and Hydrogen Halides
High-Temperature Corrosion and Materials Applications
High-Temperature Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Stress-Assisted Corrosion and Cracking
High-Temperature Corrosion and Materials Applications
High-Temperature Corrosion in Gasifiers
Corrosion: Environments and Industries
Corrosion of Nickel and Nickel-Base Alloys
Corrosion: Materials
High-Temperature Corrosion-Related Failures
Failure Analysis and Prevention (2021 Edition)
High-Temperature Corrosion in Waste-to-Energy Boilers
Corrosion: Environments and Industries
Corrosion in High-Temperature Environments
Corrosion: Environments and Industries