Chapter 1: Introduction
-
Published:2007
Abstract
This chapter outlines the topics covered in the book and explains why and to whom the book was written. The book is intended for engineers, metallurgists, and failure analysts who work with materials and components that operate in high-temperature corrosive environments. It covers eight basic modes of high-temperature corrosion as well as the effect of external and residual stresses. It also provides an extensive amount of engineering data associated primarily with commercial alloys.
Topics
Stress-induced corrosion,
High-temperature corrosion,
Erosion corrosion,
Stress corrosion cracking,
Liquid metal embrittlement,
Steel,
Boilers,
Incinerators and incineration equipment,
Waste-heat recovery systems,
Fuel-fired furnaces,
Recovery boilers,
Liquor processing and handling equipment,
Ferrous metals and alloys,
Nonferrous metals and alloys
You do not currently have access to this chapter.
Citation
Introduction, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 1, https://doi.org/10.31399/asm.tb.htcma.t52080001
Download citation file:
Related Book Content
Registered Trademarks and Trademarks
High-Temperature Corrosion and Materials Applications
Challenges in Materials Applications for High-Temperature Service
High-Temperature Corrosion and Materials Applications
Corrosion by Halogen and Hydrogen Halides
High-Temperature Corrosion and Materials Applications
High-Temperature Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Stress-Assisted Corrosion and Cracking
High-Temperature Corrosion and Materials Applications
High-Temperature Corrosion in Gasifiers
Corrosion: Environments and Industries
Corrosion of Nickel and Nickel-Base Alloys
Corrosion: Materials
High-Temperature Corrosion-Related Failures
Failure Analysis and Prevention (2021 Edition)
High-Temperature Corrosion in Waste-to-Energy Boilers
Corrosion: Environments and Industries
Corrosion in High-Temperature Environments
Corrosion: Environments and Industries