Chapter 14: The Failure Analysis Process
-
Published:2012
Abstract
This chapters discusses the basic steps in the failure analysis process. It covers examination procedures, selection and preservation of fracture surfaces, macro and microfractography, metallographic analysis, mechanical testing, chemical analysis, and simulated service testing.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
The Failure Analysis Process, Fatigue and Fracture: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 549–583, https://doi.org/10.31399/asm.tb.ffub.t53610549
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Use of Fractography for Failure Analysis
Metals Handbook Desk Edition (2nd Edition)
Fatigue Fracture Appearances
Failure Analysis and Prevention
Failure Analysis of Stress-Corrosion Cracking
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Examination Methods
Failure Analysis of Engineering Structures Methodology and Case Histories
Metallographic Technique for Nonferrous Metals and Special-Purpose Alloys
Metals Handbook Desk Edition (2nd Edition)
Metallographic Techniques for Tool Steels
Metallography and Microstructures
Metallography and Microstructures of Stainless Steels and Maraging Steels
Metallography and Microstructures
Practices in Failure Analysis
Failure Analysis and Prevention
Metallography and Microstructures of Cast Iron
Cast Iron Science and Technology
Introduction to Failure Analysis
Composites