Fatigue and Fracture: Understanding the Basics
Chapter 4: Fracture Mechanics
-
Published:2012
Abstract
Fracture mechanics is the science of predicting the load-carrying capabilities of cracked structures based on a mathematical description of the stress field surrounding the crack. The fundamental ideas stem from the work of Griffith, who demonstrated that the strain energy released upon crack extension is the driving force for fracture in a cracked material under load. This chapter provides a summary of Griffith’s work and the subsequent development of linear elastic and elastic-plastic fracture mechanics. It includes detailed illustrations and examples, familiarizing readers with the steps involved in determining strain energy release rates, stress intensity factors, J-integrals, R-curves, and...
Sign in
ASM members
Member Sign InFracture Mechanics, Fatigue and Fracture: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 101–145, https://doi.org/10.31399/asm.tb.ffub.t53610101
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.