Case 45: Failure of a Cooling Fin in an Aircraft Engine
-
Published:2005
Abstract
During a routine preflight inspection of a piston aircraft engine, part of a cooling fin was found that had broken off the cylinder. The piece, made of aluminum-silicon alloy, was cleaned and examined. Based on the fracture characteristics revealed by an electron microscope, it was concluded that the fin failed in a brittle manner by overload.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Failure of a Cooling Fin in an Aircraft Engine, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 172, https://doi.org/10.31399/asm.tb.faesmch.t51270172
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Failure of Tail Boom Attachments in a Helicopter
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Quill Shaft
Failure Analysis of Engineering Structures Methodology and Case Histories
Cracking of the Skin in the Main Rotor Blade in a Helicopter
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Nose Undercarriage Retraction Jack Support Beam
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Connecting Rod Bolts in a Ground-Based Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Max Screws in Fuel-Injection Pumps
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a First-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of an Aileron Control Cable in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure Analysis of a Cracked Gasoline Engine Cylinder Head
Handbook of Case Histories in Failure Analysis
Failure Analysis of Spline Shaft in Beco Lathe
Handbook of Case Histories in Failure Analysis