Case 28: Failure of Shutter Bolts in a Reaction Control Valve in an Aircraft
-
Published:2005
Abstract
An aircraft crashed following the loss of yaw control in full airborne flight. The subsequent discovery of broken shutter bolts in the rear pitch reaction control valve led to an inspection campaign that found bolt failures of a similar nature in valves on several other aircraft. The bolts were removed and analyzed to determine the mode and cause of failure. Based on the results of macroscopy, scanning electron fractography, metallographic examination, and chemical analysis, the failures were caused by stress corrosion cracking, and in one case, overtightening.
Sign in
ASM members
Member Sign InFailure of Shutter Bolts in a Reaction Control Valve in an Aircraft, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 130–132, https://doi.org/10.31399/asm.tb.faesmch.t51270130
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.