Abstract
Liquid penetrant, magnetic particle, and eddy current inspection are used to detect surface flaws. This chapter is a detailed account of the physical principles, process description, equipment requirements, selection criteria, advantages, limitations, and applications of these surface flaw detection techniques.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Liquid Penetrant, Magnetic Particle, and Eddy-Current Inspection, Inspection of Metals: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2013, p 183–232, https://doi.org/10.31399/asm.tb.imub.t53720183
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Inspection of Tubular Products
Inspection of Metals Understanding the Basics
Inspection of Forgings
Inspection of Metals Understanding the Basics
Inspection of Weldments and Brazed Assemblies
Inspection of Metals Understanding the Basics
Inspection of Castings
Inspection of Metals Understanding the Basics
Inspection of Steel Bar and Wire
Inspection of Metals Understanding the Basics
Visual Inspection
Metals Handbook Desk Edition (2nd Edition)
Liquid Penetrant Inspection
Nondestructive Evaluation of Materials
Nondestructive Testing in Failure Analysis
Failure Analysis and Prevention (2021 Edition)