Abstract
Visual inspection is the most important method of inspection of materials. This chapter describes the procedures involved in visual inspection such as identification markings, identification of defects caused by heating problems, scaling of materials, cracking characterization, and measurement of material dimensions. It discusses the mechanisms, advantages, limitations, components, and applications of various visual inspection tools, namely magnifying devices, lighting for visual inspection, measuring devices, miscellaneous measuring equipment, record-keeping devices, and macroetching.
Sign in
ASM members
Member Sign InVisual Inspection, Inspection of Metals: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2013, p 21–47, https://doi.org/10.31399/asm.tb.imub.t53720021
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.