Chapter 11: Opportunities for Powder-Binder Forming Technologies
-
Published:2020
Abstract
This chapter is intended to identify materials, processes, and designs that will lead to great advances in powder-binder forming technologies. It discusses some of the structures obtained through these advances in powder-binder technologies such as binder jetting and extrusion-based additive manufacturing, including bound-metal deposition and fused-filament fabrication: oxidation-resistant high-temperature alloys, anisotropic structures, submicrometer-scale structures, surface hard materials, and artist metallic clays. Some of the advances discussed include the developments in process involving plastics, emulsions, ceramics, and porous structures and foams. Improvements in the design processes have led to the development of functional structures, controlled porosity, and bioinspired structures.
Sign in
ASM members
Member Sign InOpportunities for Powder-Binder Forming Technologies, Binder and Polymer Assisted Powder Processing, By Randall M. German, Animesh Bose, ASM International, 2020, p 251–260, https://doi.org/10.31399/asm.tb.bpapp.t59290251
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!